This consists for the most part in straightening up, cleaning, and, on thicker plates above 5/16 in vee-ing the edges . 主要是矫直,清选,对于厚度超过516英寸的金属板,还需将焊边做成V形坡口。
Some crack extension probably developed from the unfused section of the butt weld across the thickness of the stiffener during transport and erection . 有些裂纹可能在运输和安装过程中就从加劲肋对接焊未熔透处开始发展。
Cell connectors and terminal post burning must be done in such a manner that there is complete fusion of the post strap top and the cover lead bushing with the connector ring or terminal post . 连接条和接线柱的焊接必须使极柱顶部和盖子的铅衬套与连接条环口或接线柱完全熔焊牢固。
Code of practice for validation of arc welding equipment 电弧焊设备验证实用规程
Symbol and notation for brazing , soldering and sealing 钎焊封接的代号及标注方法
Development of flux - cored wire for sa213 - t91 steel tig welding 焊药芯焊丝的研制
Good morning , tim . - good morning , mr . bigweld , sir 早安,提姆-早安,大焊先生
The development of bead welding rods for corrugated roller 瓦楞辊堆焊焊条的研制
Repair welding of bolting material is not permitted 螺栓材料的补焊是不允许的。